BRILLIANT CORE COATING COMPOSITION
SOURCE: Shimizu [1], page 219.
COMMENTS: This composition can be used to prime the "Brilliant Core Star." Roll the cores in this prime until they are round.
PREPARATION (parts by weight):
CHEMICAL | PERCENT/PARTS | AMOUNT |
Potassium perchlorate | 0.330 | |
Barium nitrate | 0.340 | |
Aluminum (fine flake) | 0.100 | |
Rosin (BL combustion agent) | 0.080 | |
Antimony trisulfide OR sulfur | 0.090 | |
Boric acid | 0.010 | |
Soluble glutinous rice starch | 0.050 | |
Total |