DELAY COMPOSITION #2
SOURCE:Kirk-Otthmer technical encyclopedia [8], "Explosives and Propellants"
COMMENTS: Heat of reaction: 2.081 kJ/g; gas volume: 12 cm3/g; ignition temperature: 485°C; impact sensitivity test: 23% of TNT.
PREPARATION (parts by weight):
| CHEMICAL | PERCENT/PARTS | AMOUNT |
| Barium chromate | 0.600 | |
| Zirconium-nickel alloy | 0.260 | |
| Potassium perchlorate | 0.140 | |
Total | ||