« Back Main Next » Print




GREEN STAR #2

COMMENTS: This composition leaves lots of ash. Adding ammonium perchlorate improves this.

PREPARATION (parts by weight):

CHEMICALPERCENT/PARTSAMOUNT
Barium nitrate0.500
Lab-grade magnesium powder0.320
Parlon OR PVC0.180
Total


Mix parlon with magnesium. Ad 50 volume parts of acetone, mix well and mix in the other ingredients. If PVC is used, add the correct amount of the solution in THF to the other ingredients.